We offer 2" LiNbO3 wafers with the following common specification
Crystal: LiNbO3
Working surface normal to Y-axis (+/-0.30 deg)
Diameter: 50.8 mm (+/-0.5 mm)
Thickness: 0.175 mm (+/-0.020 mm)
Flatness: TTV <= 7 microns;
LTV (5x5mm2; 95%; 2mm edge exclusion) <= 1.5 microns
Warp: <= 40 microns
Curie Temperature: 1133 - 1145°C (+/- 3 °C)
Frontside: Mechano-chemical mirror polished; No pits or scratches
Backside: Ra = 0,2 - 0,7 microns 
Flat length: 32.0 mm (+/- 3 mm)
Flat orientation: perpendicular to Z axis (+/-0.30 degrees)
Edges: All edges rounded
 